Mechanical Properties Metric English Comments
1% Secant Modulus, TD 101 MPa
14600 psi
ASTM D882
ExxonMobil Escorene® LD 713.93 Cast Film Resin
Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhbits very high impact strength, hihg clarity, and excellent heat sealabilityAvailability: Latin..