Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 883 MPa | 128000 psi | 1 in/min; ASTM D882 |
Total HDPE 6420 High Density Polyethylene, Film Resin Polyethylene: Medium molecular weight, high density film resinCharacteristics:Excellent moisture barrier propertiesLow gelsLow taste and odorHigh stiffnessGood processabilityGood compatibility with.. |