1% Secant Modulus, TD 117 MPa
17000 psi
ASTM D882
ExxonMobil LDPE LD 319.92 Low Density Polyethylene Resin
Product Description: LD 319.92 resin is an 8.7% vinyl acetate copolymer film resin. Film made from LD 319.92 exhibits superior impact strength and heat sealability.Availability: Latin America, North..