Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 614 MPa | 89000 psi | ASTM D882 |
Chevron Phillips mPact™ D449 HDPE Blown Film Resin
(discontinued **) Resin Type: High density, hexene copolymerCharacteristics: excellent clarity, high gloss, good modulus, process with LLDPE setup, optimum clarity when used as an individual layer.Applications: overw.. |