Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 80.0 MPa | 11600 psi | ISO 527-3 |
Polimeri Europa Clearflex® CL B0 Very Low Density Polyethylene Clearflex CL B0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has a high stretchability and a good cling effect.Main Applications: C.. |