Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 430 MPa
62400 psi
ISO 527-3
Polimeri Europa Clearflex® H&T FHH 508 Octene Copolymer Linear Medium Density Polyethylene
Clearflex H&T FHH 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidant, suitable for blown film extrusion.Films obtained from Clearflex H&T FHH 508 show good op..