Mechanical Properties Metric English Comments
1% Secant Modulus, MD 352 MPa
51000 psi
ASTM D882
ExxonMobil LDPE LD 157CW Blown Low Density Polyethylene Resin
Product Description: LD 157CW offer good mechanical properties as well as excellent opticals.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesAppl..