Polymer Property : 1% Secant Modulus, MD = 286 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 286 MPa
41500 psi
ASTM D882
ExxonMobil LL 3201.22 Premium High Strength Film Resin  (discontinued **)
LL 3201 resins are hexene copolymer LLDPE film resins. Films produced from these resins have excellent tensile, toughness and stiffness properties. These strength properties, along with good drawdow..