Mechanical Properties Metric English Comments
1% Secant Modulus, MD 215.74 MPa
31291 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF268GG Low density polyethylene
LDF268GG is a low density polyethylene resin for film extrusion. LDF268GG has medium slip and anti-block additives. LDF268GG meets the U.S. Food and Drug Administration (FDA) criteria for food conta..
1% Secant Modulus, MD 215.74 MPa
31291 psi
ASTM D882
Lotte Chemical Titan TITANLENE® LDF250YZ Low density polyethylene
LDF250YZ is a low density polyethylene resin for film extrusion. LDF250YZ has no slip and anti-block additives. LDF250YZ meets the U.S. Food and Drug Administration (FDA) criteria for food contact u..