Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 19.3 MPa | 2800 psi | ASTM D882 |
Westlake EF706 Low Density Polyethylene Westlake EF706 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound.. |