Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 119 MPa | 17300 psi | ASTM D882 |
ExxonMobil LL 3001.32 Cast Film Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |