Polymer Property : 1% Secant Modulus, MD = 134.96 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 134.96 MPa
19575 psi
ASTM D882
NOVA Chemicals Surpass® FPs117-D Octene sLLDPE Film Resin  (discontinued **)
Applications: Lamination Film, coextruded sealant layer, high toughness filmInformation provided by Nova Chemicals