Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 917 MPa | 133000 psi | ASTM D882 |
Lotte Chemical Titan TITANEX® HF1881 High density polyethylene Hexene-1 resin HF1881 is a pelleted medium molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners and thin films.Advantages: Speci.. |
|||
1% Secant Modulus, MD | 917 MPa | 133000 psi | 1 in/min; ASTM D882 |
Total HDPE HL 535 High Density Polyethylene, Film Resin Polyethylene: Medium molecular weight, high density film resinCharacteristics:High stiffnessGood heat resistanceExcellent bubble stabilityGood compatibility with LDPE and LLDPEApplications:Release .. |