Mechanical Properties Metric English Comments
1% Secant Modulus, MD 131 MPa
19000 psi
ASTM D882
ExxonMobil Exceed™ 1012CA Film Resin  (discontinued **)
Exceed 1012CA mVLDPE resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1012CA resin have outstanding cold temperature toughness, impact strength a..
1% Secant Modulus, MD 131 MPa
19000 psi
ASTM D882
LyondellBasell Petrothene® NA442051 Low Density Polyethylene
ApplicationsPETROTHENE NA 442 is a series of low density/EVA copolymer resins for high impact/high clarity packaging and lamination applications. NA 442 exhibits excellent processability and good b..
1% Secant Modulus, MD 131 MPa
19000 psi
ASTM D882
LyondellBasell Petrothene® NA480145 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
1% Secant Modulus, MD 131 MPa
19000 psi
ASTM D882
LyondellBasell Petrothene® NA480177 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
1% Secant Modulus, MD 131 MPa
19000 psi
ASTM D882
LyondellBasell Petrothene® NA480178 Low Density Polyethylene
ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low..
1% Secant Modulus, MD 131 MPa
19000 psi
ASTM D882
Westlake Elevate™ EF446 6.0% Ethylene Vinyl Acetate Copolymer
Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio..