Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 128 MPa | 18500 psi | ASTM D882 |
ExxonMobil LD 307.76 Clear, High Impact Film Resin LD 307.76 film has superior impact strength and heat sealability, used in frozen and other food packaging, and high strength bags.Information provided by ExxonMobil Chemical |