Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 11.7 MPa | 1700 psi | ASTM D882 |
ExxonMobil LL 3003.39 Cast Film Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |