Mechanical Properties Metric English Comments
1% Secant Modulus, MD 1070 MPa
155000 psi
ASTM D822
LyondellBasell Alathon® L4907 High Density Polyethylene
ApplicationsALATHON L 4907 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits high density and stiffness and is designed for gro..