Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 710 MPa @Thickness 0.0254 mm |
103000 psi @Thickness 0.00100 in |
2.5 BUR; ASTM D882A |
Total HL 428 HDPE Film Grade Medium molecular weight grade. Excellent processability, excellent compatibility with LDPE and LLDPE, good tear and impact strength, good stiffness, excellent drawdown, and good moisture barrier pro.. |
|||
1% Secant Modulus, MD | 710 MPa | 103000 psi | ASTM-D882 |
Braskem HD3000N HDPE Cast Film Extrusion Polyethylene Homopolymer HD3000N is a high-density polyethylene, narrow molecular weight homopolymer produced by the solution process for cast film extrusion. It offers high processability, stiffness, and good impact resist.. |