Mechanical Properties Metric English Comments
Flexural Yield Strength 94.5 - 267 MPa

@Temperature 100 - 175 °C
13700 - 38700 psi

@Temperature 212 - 347 °F
Average value: 158 MPa Grade Count:1
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..