Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 63.3 MPa @Thickness 6.40 mm |
9170 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron SE-32M ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |
|||
Flexural Yield Strength | 63.3 MPa @Thickness 6.40 mm |
9170 psi @Thickness 0.252 in |
ASTM D-790 |
Bhansali Engineering Abstron SE-32M ABS Sheet Extrusion Grade Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali |