Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 8960 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 61.8 MPa

@Thickness 3.20 mm
8960 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical HI100H ABS, High Impact, High Toughness
Feature: Injection Molding, High Impact, High ToughnessApplication: Helmet, Pipe & Fittings)CAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 61.8 MPa

@Thickness 3.20 mm
8960 psi

@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical HI100K ABS, High Impact
Feature: Injection Molding, High Impact, Good ProcessingApplication: Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
Flexural Yield Strength 61.8 MPa
8960 psi
ASTM D790
Iran Petrochemical (PCC) SV-0157 Acrylonitrile Butadiene Styrene
SV - 0157 ABS extrusion grade has been formulated to provide excellent mechanical properties, extrusion stability, vacuum formability and chemical resistance. It has low flow with high impact streng..
Flexural Yield Strength 61.8 MPa
8960 psi
ASTM D790
Cheng Yu Plastic PP222 Flame Retardant Polypropylene, High Impact
Flexural Yield Strength 61.8 MPa

@Thickness 6.40 mm
8960 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade
Medium Impact, High Gloss, High FlowInformation provided by Bhansali
Flexural Yield Strength 61.8 MPa

@Thickness 6.40 mm
8960 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron IMC25 ABS-PC Alloy
Medium FlowInformation provided by Bhansali
Flexural Yield Strength 61.8 MPa

@Thickness 6.40 mm
8960 psi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Flexural Yield Strength 61.8 MPa

@Thickness 6.40 mm
8960 psi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron IM-29 ABS Injection Molding Grade
High Impact, Medium, High Flow, General PurposeInformation provided by Bhansali
Flexural Yield Strength 61.8 MPa

@Thickness 6.40 mm
8960 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron IM-17A ABS Injection Molding Grade
Medium Impact, High Gloss, High FlowInformation provided by Bhansali
Flexural Yield Strength 61.8 MPa

@Thickness 6.40 mm
8960 psi

@Thickness 0.252 in
5 mm/min; ASTM D790
Bhansali Engineering Abstron IMC25 ABS-PC Alloy
Medium FlowInformation provided by Bhansali
Copyright © lookpolymers.com All Rights Reserved