Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 186 - 894 MPa | 27000 - 130000 psi | Average value: 311 MPa Grade Count:19 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |