Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 5.88 MPa @Thickness 6.40 mm |
853 psi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL ED1045D TPO, Thermoplastic Elastomer Description: Injection Molding, TPO, Thermoplastic Elastomer, Soft TouchApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0, 1333-86-4, 25087-34-7 and 14807-96-6Information provided.. |