Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 84.8 MPa | 12300 psi | ASTM D790 |
PolyOne Geon™ CPVC MC550 Polyvinyl Chloride, Chlorinated (CPVC) Information provided by PolyOne |
|||
Flexural Yield Strength | 84.8 MPa | 12300 psi | ASTM D790 |
Star Plastics ABSGF20 Molding Grade ABS With 20% Glass Information provided by Star Plastics, Inc. |