Mechanical Properties Metric English Comments
Flexural Yield Strength 83.5 MPa
12100 psi
15 mm/min; ASTM D790
LG Chemical 15NFI GPPS
High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio..