Flexural Yield Strength 54.92 MPa

@Thickness 6.40 mm
7965 psi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron SE-45 ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali
Flexural Yield Strength 54.92 MPa

@Thickness 6.40 mm
7965 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade
Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali
Flexural Yield Strength 54.92 MPa

@Thickness 6.40 mm
7965 psi

@Thickness 0.252 in
ASTM D-790
Bhansali Engineering Abstron SE-22M ABS Sheet Extrusion Grade
Sheet Extrusion grade for profile & DoorsInformation provided by Bhansali
Flexural Yield Strength 54.92 MPa

@Thickness 6.40 mm
7965 psi

@Thickness 0.252 in
ASTM D790
Bhansali Engineering Abstron SE-45 ABS Sheet Extrusion Grade
Super high and Very High Impact Sheeting grades for Automobile & Luggage ApplicationsInformation provided by Bhansali