Polymer Property : Flexural Yield Strength = 79.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 2.26 - 79.0 MPa
327 - 11500 psi
Average value: 20.1 MPa Grade Count:31
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..