Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 77.828 MPa | 11288 psi | ASTM D790 |
KKPC Kuhmo GP 125EB Extrusion Molding GPPS Key features: PSP Common Uses: Fruit, egg cell.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability, and stability of dimension.Da.. |