Mechanical Properties Metric English Comments
Flexural Yield Strength 49.2 MPa
7140 psi
ASTM D790
Devcon Combo Wear FC Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Flexural Yield Strength 49.2 MPa
7140 psi
ASTM D790
Devcon Wear Guard (High Load) Epoxy
Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives.
Copyright © lookpolymers.com All Rights Reserved