Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 70.60 MPa | 10240 psi | ASTM D790 |
TPI Porene® GA800TW High Gloss/Weather Resistant/Antistatic Grade ABS INJECTION MOLDING; ANTISTATIC; WEATHER RESISTANT. HOUSING OF ELECTRICAL APPLIANCES, e.g. ELECTRIC FAN, TELEPHONE, CALCULATOR, TOYSPorene® is a registered trademark of Thai Petrochemical Industry C.. |