Polymer Property : Flexural Yield Strength = 70.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 0.483 MPa
70.0 psi
(5% Strain) at 2 pcf expanded density; ASTM C203
NOVA Chemicals Dylite® F271T Specialty Expandable Polystyrene
Features: Highly consistent bead size; high gloss characteristics; low energy consumption; fast cyclingApplications: Drinking cups -hot and cold, noodle bowls, take-out and ice cream containers, and..