Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 64.1 MPa | 9300 psi | ASTM D790 |
Star Plastics ABSFR1 Molding Grade ABSFR Information provided by Star Plastics, Inc. |
|||
Flexural Yield Strength | 64.1 MPa | 9300 psi | ASTM D790 |
Star Plastics ABSFR2 Molding Grade ABS Information provided by Star Plastics, Inc. |