Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 47.1 - 579 MPa | 6830 - 84000 psi | Average value: 73.4 MPa Grade Count:112 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |