Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 57.8 MPa
8380 psi
ASTM D790
Samsung Cheil Industries Starex® VH-0850 ABS, Unreinforced  (discontinued **)
Amorphous Acrylonitrile Butadiene Styrene (ABS)Characteristics: Flame Retardant: Balance of Properties (Impact, Mechanical and Heat)Applications: Computer, Monitor and Printer Housings, Microwave Co..