Mechanical Properties Metric English Comments
Flexural Yield Strength 39.2 - 88.9 MPa
5690 - 12900 psi
Average value: 72.0 MPa Grade Count:16
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Flexural Yield Strength 39.2 MPa

@Thickness 3.20 mm
5690 psi

@Thickness 0.126 in
15mm/min; ASTM D790
LG Chemical HIPS 410AF PS, Flame Retardant
Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical
Flexural Yield Strength 39.2 MPa

@Thickness 6.40 mm
5690 psi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL GP3202B PP+MF20%
Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Flexural Yield Strength 39.2 MPa

@Thickness 6.40 mm
5690 psi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL GP3202Z PP+MF20%
Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Electrical, Electronic and Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical
Flexural Yield Strength 39.2 MPa

@Thickness 6.40 mm
5690 psi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL HI5205 PP+MF20%, High Impact
Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical
Flexural Yield Strength 39.2 MPa

@Thickness 6.40 mm
5690 psi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL HI5302R PP+MF30%, High Impact
Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Flexural Yield Strength 39.2 MPa

@Thickness 6.40 mm
5690 psi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL HI5302RB PP+MF25%, High Impact
Description: Injection Molding, PP+MF25%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical
Flexural Yield Strength 39.2 MPa
5690 psi
ASTM D790
KKPC Kuhmo HF 430U Weather-resistant Flame Retarded HIPS
Key features: Excellent weather-resistance, non-deca heat-resistance. Common Uses: TV and VCR housing, parts needing non-deca type.HIPS is a functional resin made by copolymerization of styrene mono..
Flexural Yield Strength 39.2 MPa

@Thickness 6.40 mm
5690 psi

@Thickness 0.252 in
10mm/min; ASTM D790
LG Chemical LUPOL TE5007B PP+Rubber, High Impact
Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical
Flexural Yield Strength 39.2 MPa
5690 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled
Information from Shinkong Synthetic Fibers Corp.
Flexural Yield Strength 39.2 MPa
5690 psi
ASTM D790
Cheng Yu Plastic PE221 Flame Retardant LDPE
Flexural Yield Strength 39.2 MPa
5690 psi
ASTM D790
Cheng Yu Plastic BK1020 Electric Conducting LDPE
Flexural Yield Strength 39.2 MPa
5690 psi
ASTM D790
Shinkong Synthetic Fibers Shinite® P301T20 PP, 20% Talc Filled
Information from Shinkong Synthetic Fibers Corp.