Polymer Property : Flexural Yield Strength = 56500 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 120 - 390 MPa
17400 - 56500 psi
Average value: 278 MPa Grade Count:24
Overview of materials for Polyarylamide, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values..