Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 37.9 - 75.0 MPa | 5500 - 10900 psi | Average value: 56.4 MPa Grade Count:10 |
Overview of materials for Nylon 12, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Flexural Yield Strength | 37.9 MPa | 5500 psi | ASTM D790 |
Spartech Royalstatâ„¢ R64 HDPE Static Control Sheet Description: Static Control SheetInformation provided by Spartech. |
|||
Flexural Yield Strength | 37.9 MPa | 5500 psi | ASTM D790 |
Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber Data provided by Clariant Masterbatches |