Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 125 - 375 MPa | 18100 - 54400 psi | Average value: 211 MPa Grade Count:32 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |