Mechanical Properties Metric English Comments
Flexural Yield Strength 352 MPa
51000 psi
ASTM D790
Techmer ES Electrafil® J-1/CF/30 Nylon 66, 30% Carbon Fiber Reinforced
Carbon Fiber Reinforced
Flexural Yield Strength 352 MPa
51000 psi
ASTM D790
Techmer ES Plastiblend® PA6/6,6 GF60 HS L 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat..