Mechanical Properties Metric English Comments
Flexural Yield Strength 344 MPa
49900 psi
ASTM D790
Quantum Composites QC-8151C 55% Glass Fiber Vinyl Ester Static-Dissipative SMC  (discontinued **)
QC-8151C is a vinyl ester sheet molding compound (SMC) designed for compression molding components requiring dimensional stability, resistance to high temperatures plus sufficient electrical conduct..
Flexural Yield Strength 344 MPa
49900 psi
ASTM D790
Quantum Composites QC-8770 63% Glass Fiber Hybrid Vinyl Ester SMC  (discontinued **)
QC-8770 is a hybrid vinyl ester-based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and excellent st..