Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 103 - 331 MPa | 15000 - 48000 psi | Average value: 244 MPa Grade Count:34 |
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values.. |