Polymer Property : Flexural Yield Strength = 432 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 432 MPa
62700 psi
ASTM D790
Covestro Baydur® STR/C-400 BB Polyurethane Composite SRIM Foam, 60% Glass Filled, MDI-based 2-Component Liquid System
Contains directed chopped fiber preform glass.0.16 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bay..