Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 43.49 MPa | 6308 psi | ASTM D790 |
KKPC Kuhmo HI 420T Transparent HIPS Key features: Translucent Extrusion. Common Uses: Transparent toys, glass cases, various products made by injection molding needing contact-movability.HIPS is a functional resin made by copolymeriza.. |
|||
Flexural Yield Strength | 43.49 MPa | 6308 psi | ASTM D790 |
KKPC Kuhmo MIB 237 Blow Molding HIPS Key features: Good-profiling, Thin-layer Molding. Common Uses: It is used exclusively as a container for fermented milk beverages.HIPS is a functional resin made by copolymerization of styrene monom.. |