Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 155 - 290 MPa | 22500 - 42000 psi | Average value: 214 MPa Grade Count:15 |
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an.. |
|||
Flexural Yield Strength | 84.1 - 290 MPa | 12200 - 42000 psi | Average value: 198 MPa Grade Count:36 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |