Mechanical Properties Metric English Comments
Flexural Yield Strength 42.7 MPa
6190 psi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 8% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Flexural Yield Strength 42.7 MPa
6190 psi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 8% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Flexural Yield Strength 42.7 MPa
6190 psi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 8% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Flexural Yield Strength 42.7 MPa
6200 psi
ASTM D790
Westlake Plastics HIPS High Impact Polystyrene, Compression Molded
Compression molded HIPS is a low cost plastic material that is easily machined and fabricated. It is frequently used for preproduction prototyping. HIPS is a FDA compliant use in food processing a..
Flexural Yield Strength 42.7 MPa
6200 psi
ASTM D790
Westlake Plastics HIPS High Impact Polystyrene
HIPS is a low cost plastic material that is easy to machine and fabricate. It is often specified for low strength structural applications when impact resistance, machinability, and low cost are req..
Flexural Yield Strength 42.7 MPa
6190 psi
ASTM D790
Eastman Tenite Butyrate 465A3720010 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 10%. Weight loss on heating = 0.9% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..