Polymer Property : Flexural Yield Strength = 41800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 288 MPa
41800 psi
ASTM D790
Solvay Specialty Polymers Kadel® E-1300 Polyketone  (discontinued **)
High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical r..
Flexural Yield Strength 288 MPa
41800 psi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Verton RV008ESV PA 66
40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region.