Polymer Property : Flexural Yield Strength = 370 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 9.65 - 370 MPa
1400 - 53700 psi
Average value: 151 MPa Grade Count:233
Overview of materials for Nylon 6, Heat Stabilized
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro..
Flexural Yield Strength 110 - 370 MPa

@Temperature -40.0 - 120 °C
16000 - 53700 psi

@Temperature -40.0 - 248 °F
Average value: 240 MPa Grade Count:1
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Flexural Yield Strength 62.1 - 370 MPa
9000 - 53700 psi
Average value: 188 MPa Grade Count:43
Overview of materials for Polypropylene, Long Glass Fiber 50%
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include..