Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 368 MPa | 53400 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66 LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive. |