Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 360 MPa | 52200 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP RC006 PA6.6 (Europe-Africa-Middle East) LNP* THERMOCOMP* RC006 is a compound based on PA6.6 resin containing Carbon Fiber. Added features include: Electrically Conductive. |