Mechanical Properties Metric English Comments
Flexural Yield Strength 231 MPa
33500 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP EF006E PEI
LNP THERMOCOMP* EF006E is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
Flexural Yield Strength 231 - 360 MPa
33500 - 52200 psi
Average value: 299 MPa Grade Count:33
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40%
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. ..